Solder Ball | 20 May, 2013

What is the effect of Ni in SAC Solder Ball?

reply »

#69002

Solder Ball | 20 May, 2013

SAC / Ni interface is the IMC (Cu, Ni)6Sn5

reply »

#69013

Solder Ball | 20 May, 2013

So u mean it is to form the intermetallic compound which is (Cu,Ni)6Sn5?

reply »

#69018

Solder Ball | 21 May, 2013

yes