ESD Epoxy flooring | 19 June, 2013

Does anyone have any input on ESD Epoxy flooring, positive or negative?

reply »

#69404

ESD Epoxy flooring | 19 June, 2013

I've used it at my last two companies, and quite like it. The base floor has to be prepared correctly, so that the epoxy bonds correctly, but, it's easy to maintain, and is pretty durable.

Repeated movement of bench chairs over it does cause wear, though; especially when you introduce lead clippings, etc; but, it's pretty easy to touch up.

Cheers, ..rob

reply »

#69410

ESD Epoxy flooring | 19 June, 2013

were you forced to reapply over time? thanks for the input.

reply »

#69413

ESD Epoxy flooring | 19 June, 2013

We only reapplied in areas where significant wear was observed. As I mentioned, shop chairs moving back and forth, combined with lead trimmings and other debris led to scraping and peeling over time.

Other than that, no, we did not re-apply over time.