ERSA users 1.8/2.5 nozzle | 14 November, 2013

Recently, we have been experimenting with the 1.8/2.5 nozzle to be able to solder leads that are near an SMD. This pcbs were not design for selective solder, so we are trying to work within this limitations.

I found the 1.8 nozzle very hard to install at start up, solder has the tendency to stop flowing and get cold at the top, so makes it impossible to do a wave height test. Time spent getting this nozzle to work is ridiculous.

I don't want to give up yet on this one, but it is sure frustrating.

reply »

#71394

ERSA users 1.8/2.5 nozzle | 14 November, 2013

We use a 2mm with our Pillarhouse Jade Mark II. We found that reducing the nitrogen enough that the area around the nozzle stays hot enough not to "freeze".

reply »

#71397

ERSA users 1.8/2.5 nozzle | 15 November, 2013

Thanks for the pointer tombstonesmt, I'll give that a shot. Being able to utilize this nozzle will help tremendously. I'll post results as they become available.