VIGON A200 and aluminium electrolytic capacitors problem | 21 November, 2013

Hello,

We've just started using VIGON A200 in our Aqueous Trident XLD system and observed that aluminium electrolytic capacitors get corroded.

Concentration was set at 20% and washing is done by spray at 150F for 6 to 8 minutes. Then is rinsed several times and dryed.

Any advice on this matter is most welcomed!

Thanks

reply »

#71415

VIGON A200 and aluminium electrolytic capacitors problem | 21 November, 2013

The last time I got corroded parts out of my wash was when my DI tanks were spent, and I was pretty much using straight tap water. Refreshing the DI tanks eliminated my issue.

Hope this helps.

cheers, ..rob

reply »

#71416

VIGON A200 and aluminium electrolytic capacitors problem | 21 November, 2013

Thanks for the tip!

The DI tanks are brand new.

Water quality is pretty good. The filtering is also good and the instrument in the water recycler measures about 12MOhm resistivity.

Cheers, Luciano.

reply »

#71424

VIGON A200 and aluminium electrolytic capacitors problem | 25 November, 2013

Are you using zestron corrision inhibiter Ci20 also?

reply »

#71428

VIGON A200 and aluminium electrolytic capacitors problem | 26 November, 2013

Hi!

I haven't found any info about that product. I can't even find it among Zestron products. Could you tell me where to find some info about it?

Thanks!

reply »

#71429

VIGON A200 and aluminium electrolytic capacitors problem | 26 November, 2013

Hi, Its a zestron product which we have used for many years, speak with Zestron and i m sure they will assist.

reply »

#71438

VIGON A200 and aluminium electrolytic capacitors problem | 27 November, 2013

Thanks!

reply »

#71452

VIGON A200 and aluminium electrolytic capacitors problem | 3 December, 2013

Insure your rinses are only 25 to 30-seconds each. Also there are options for cleaning solutions from Kyzen that are safer on AL and do not require dosing of any additional inhibitors.

reply »

#71468

VIGON A200 and aluminium electrolytic capacitors problem | 6 December, 2013

Thanks for the advice!