We installed a Soltec Delta 3 a few months ago and have been trying to run with a VOC free no clean. We're using SN100C in the pot. We are spraying the material and have top/bottom preheat.

Evaporation of the water in the flux is a bit of a struggle when setting up new profiles but no matter what we do, there is still some level of solder balls/fines on a given board. IPC 610 section 5.2.7.1 provides for somewhat of an out for this condition but I'm not comfortable hanging my hat on it.

We have no customer mandate to run VOC free and I'm considering a change to an alcohol based NC. Has anyone been down this road and/or tried the Kester 985M?

Thanks,

Hoss

reply »

#71430

Kester 985M - Will It Help? | 26 November, 2013

Any alcohol based flux will outperform a water based (VOC free) flux. If one thing I learned in my 35+ years in the electronics industry "Water and electronics is a bad combination".

Patrick

reply »

#71431

Kester 985M - Will It Help? | 26 November, 2013

Patrick,

Thanks for the reply and well said.

Joe

reply »

#71432

Kester 985M - Will It Help? | 26 November, 2013

Joe,

And lead FREE in combination with voc FREE is a cocktail for disaster. And it surely ain't FREE (if you know what I mean):-).

reply »

#71433

Kester 985M - Will It Help? | 26 November, 2013

OK. Now I understand. The FREE's cancel each other out.