stranded copper wire - tin or not tinned | 23 January, 2014

Should stranded copper wire (20 gauge 19 strand) be tinned prior to insertion into screw connector? One of our customers "suggests" tinned, but past experience tells us no.

reply »

#71626

stranded copper wire - tin or not tinned | 23 January, 2014

Even for me its a No. Its quiet strange why some preferred tinned ones.

reply »

#71630

stranded copper wire - tin or not tinned | 23 January, 2014

I agree with AFlex. Don't tin stranded wire that's assembled into a screw terminal block. I believe the reasoning has to do with avoiding stress on the wire metal caused by different expansion rates of the solder and the wire.