J STD 002 Test S source of ceramic substrate | 5 May, 2014

Hi, I was wondering if there is a preferred source of the .635mm ceramic substrate specified in the J STD 002 Test S and if there is what is the typical size folks are using (3" x 3"?). Thanks, Rich

reply »

#72083

J STD 002 Test S source of ceramic substrate | 6 May, 2014

Most ceramic you'll see comes from Coors or Kyocera.

Size of your substrate will vary according to the stencil / component that you're using. 3" by 3" should be sufficient for most applications. If you get them too small, you could have handling issues.

BR ... davef