Hello all!
For my mechanical engineering study I want to ...
- May 14, 2014
by
Julian
You should look in to this document:
IPC/JEDEC-9704A
Pri...
- May 14, 2014
by
tmo
Tmo,
Thanks for your reply. It gives good advise about ho...
- May 15, 2014
by
Julian
I always made tests with gauges on top or bottom surface of ...
- May 15, 2014
by
tmo
Interesting.
How did you connect the gauges in the press? O...
- May 16, 2014
by
Julian
I hate to say this but in all probability this wont work.
I...
- May 17, 2014
by
sarason
Thanks for your reply Sarason. I'm aware now that my goals s...
- May 26, 2014
by
Julian
Damn near impossible. You need to see a real change in the d...
- May 26, 2014
by
sarason