help vitronics soltec reflow ppm reach 10014 | 18 August, 2014

Hi guys. Kindly help me on our reflow (vitronics soltec). My problem is the n2 value reach 10014...any possible solution or suggestion guys..

reply »

#72585

help vitronics soltec reflow ppm reach 10014 | 18 August, 2014

Hi guys. Kindly help me on our reflow (vitronics soltec). My problem is the n2 value reach 10014...any possible solution or suggestion guys..

reply »


JD

#72707

help vitronics soltec reflow ppm reach 10014 | 8 September, 2014

We resolved this issue a few weeks ago. It was a configuration mismatch in the oven (MR933+)software with the onboard O2 analyzer.

reply »

#72710

help vitronics soltec reflow ppm reach 10014 | 8 September, 2014

Right sir we already fix it by loading configuration from other machine