conformal coating | 16 April, 2015

Anyone aware of an acrylic conformal coating that is UV curable?

reply »

#73813

conformal coating | 17 April, 2015

#73817

conformal coating | 17 April, 2015

Thanks for the info Sarason. The UVCL is a Urethane. Did not want that hard of finish (for solder rework issues). We like the Acrylic as acetone will remove cured material for solder rework.

reply »

#73821

conformal coating | 17 April, 2015

Humiseal says, "UV cure – These materials are also more difficult to repair as they are the most chemically resistant and mechanically tough of all conformal coatings. Removal is possible locally by using powder abrasion."