Topaz-Xii Error Code 30 | 24 April, 2015

I have checked and rechecked all my dimensions on the capacitor which is a 402 size. The manual says that the center is incorrect. Need some help to figure out why it is throwing this part away seeing it passes a vision test. Any help would be grateful.

Thanks Chris

reply »

#73840

Topaz-Xii Error Code 30 | 24 April, 2015

- Clean nozzles. - Clean camera. - Adjust lighting. - Check tolerance level. Good luck.

reply »

#73843

Topaz-Xii Error Code 30 | 27 April, 2015

Is it failing due to Vaccuum level?

reply »

#73845

Topaz-Xii Error Code 30 | 27 April, 2015

When I do the adjust to make sure the vision and tolerance is working it works perfectly. But if the machine runs a board I am riddled with this. I have checked the vacuum levels on all the heads and they are within where they are supposed to be for the parts it is having problems with. What kills me is Saturday it ran for 6-7 hours flawlessly having 3-4 pickup errors per board of over 900 parts. Then the last few hours it ran it was a nightmare.

Thanks Chris

reply »

#73847

Topaz-Xii Error Code 30 | 28 April, 2015

Just check that the Vacuum check is on normal and not set to Special Check.