Is anyone conformal coating flex circuits?

Views: 2595

#74160

Is anyone conformal coating flex circuits? | 1 July, 2015

I have a customer that is requesting their flex circuit be conformally coated. Is this something that is done? Which coating would stand up to the stresses of flexing? Wouldn't that put stress on the components? Thanks! Shannon

reply »


CPI

#74273

Is anyone conformal coating flex circuits? | 24 July, 2015

have done it in the past, used silicon as it will flex,, however its not the most robust material! tends to peel/flake off.

reply »

#74290

Is anyone conformal coating flex circuits? | 29 July, 2015

How many times does it have to flex. There are acrylic conformal coatings that can be bent once to 90 degrees or so

reply »


Lou

#74515

Is anyone conformal coating flex circuits? | 8 September, 2015

Commonly done with Parylene.

reply »