Guys, i hope you can help me in finding the reason why DUT p... - Sep 15, 2016 by souldierAnn
souldierAnn
#76359
DUT pad wearing out | 15 September, 2016
Guys, i hope you can help me in finding the reason why DUT pad like the photo attached had wearing out.
Highlighted in RED is the wearing out issue.