No Clean flux with more solids

Views: 2222

#77173

No Clean flux with more solids | 2 March, 2017

Hello,

I am looking for a NC flux that has more solids. Anybody using anything that has at least 7-8% solids contents?

reply »

#77174

No Clean flux with more solids | 2 March, 2017

Our Senju Sparkle Flux contains 8% solids and is a NC.

reply »

#77176

No Clean flux with more solids | 2 March, 2017

Would you specify a part number?

reply »

#77180

No Clean flux with more solids | 3 March, 2017

What kind of flux you looking for water based, alcohol based, or solvent based

reply »

#77182

No Clean flux with more solids | 3 March, 2017

Both Alcohol and Water based should work. I will try to stay away from Rosin/Resin because of the residue - issues in ICT.

reply »

#77192

No Clean flux with more solids | 6 March, 2017

The one i've been using on some thermally diverse boards with great success has been henkel loctite mfr 301. It's alcohol based not quite the solids you are looking for but close it's 5.5-6.5 solids and it is no clean.

reply »

#77203

No Clean flux with more solids | 7 March, 2017

Thank you bruce! I tried similar rosin based 6.5% but it gives me a lot of residue. Anything water based?