Argon Tank for Plasma Treatment

Views: 1011

#79289

Argon Tank for Plasma Treatment | 3 November, 2017

Hello,

I am currently in the process of purchasing a plasma chamber for the purpose of activating the surface of flex circuits so that they bond more readily. In addition I need to purchase a gas cylinder for the chamber, specifically one that is a mix of argon and oxygen, but I do not have any knowledge of what the correct gas is. Can anyone please give me some guidance on where to find this kind of gas tank?

Thanks.

reply »

#79297

Argon Tank for Plasma Treatment | 6 November, 2017

I'm a Rep for Nordson March plasma system. Here is what we recommend for the ProVIA systems; O2 = 99.996%; N2 = 99.99%; Ar = 99.999%; H2 = 99.999%