Samtec SEMA Solder Charge Connector | 16 November, 2017

I am curious to know anyone has used Samtec SEMA Solder Charge connector (SEARAY Seriese. I have done manufacturer's recommended solder paste and good reflow profile still the solder is leaching to the lead instead of becoming a solder connection.