CSP assembly compliance to IPC-A-610 minimum electrical clearance

Views: 780

#81038

CSP assembly compliance to IPC-A-610 minimum electrical clearance | 12 September, 2018

Hi,

Is the IPC-A-610 applicable to CSP assemblies? Especially regarding the solder ball to solder ball distance versus the minimum electrical clearance for assembly(0.13mm/IPC-A-610). With a 0.4mm pitch component and 260 microns diameters balls, this min. clearance seems difficult to achieve...