Kiss selective solder flux

Views: 2100

#81913

Kiss selective solder flux | 7 February, 2019

Hi All,

What are you running for selective solder flux?

I'd like any opinion on water soluble and/or no-clean fluxes you are using.

In our Kiss 104 machine we use HYDRO-X20 water soluble flux, per the original install suggestion, but I'd like to know if that is still the suggested material and if anyone has an opinion/suggestion for same/different flux.

thanks!

reply »

#81915

Kiss selective solder flux | 8 February, 2019

BLT 31-41 "No Clean Selective Flux For Aerospace" On a Versaflow 3/45

Atomises well, good hole penetration, good wetting, cleans off well in the solvent cleaner. Use for SN100C, SA0307, and 60/40.

reply »

#81964

Kiss selective solder flux | 13 February, 2019

I personally prefer a NC process if I have to chose. AIM flux was good NC377 I think(they keep changing names), NF 372 from and many more. You can make them all work...the KISS 104 ...

reply »

#82207

Kiss selective solder flux | 22 March, 2019

I believe that NORDSON now recommends AIM NC277. Nordson bought out ACE-protech.

reply »

#82208

Kiss selective solder flux | 22 March, 2019

Thank you ProcEng1

Nordson sent me a flux suggestion list:

No Clean: 1. Kester Select 10 2. ALPHA EF-2210 3. AIM FX-16

Water Sol: KESTER 2331-ZX