Is TS-2414 insulating varnish material suitable for conformal coating of PCBAs? How can its performance be tested? What properties should be looked for on its data specs to conduct initial assessment if it is a suitable coating material?

reply »

#83124

TS-2414-V Insulating Varnish | 1 August, 2019

Look at:

* Conformal Coating 101 - https://www.smta.org/chapters/files/UpperMidwest_BTW_Conformal_Coating_June_27th_2012.pdf

* IPC Conformal Coating Course - https://edge.ipc.org/course/conformal-coating

* IPC-CC-830: Qualification and Performance of Electrical Insulating Compound for Printed Wiring Assemblies

* IPC-HDBK-830: Guidelines for Design, Selection and Application of Conformal Coatings