I am having trouble with achieving wetting on fences and I c... - Aug 07, 2019 by QA123
We do this often. Including fences with many internal struct... - Aug 08, 2019 by SMTA-Joe SMTA
I am placing these at SMT.... they are going through reflow ... - Aug 08, 2019 by QA123
Ok, interesting. Unfortunately I can't speak on that. We alw... - Aug 08, 2019 by SMTA-Joe SMTA
Thanks for the feedback I will pull a group together and dis... - Aug 08, 2019 by QA123