What flux are you using for spray/ dropjet (Selective Solder) | 13 November, 2019

We've been using AIM NC277 in our dropjet fluxers. Well it's discontinued.

I've talked to the manufacturer and got what they recommend. I'm wondering what anybody else is using that they are happy with.

reply »

#83811

What flux are you using for spray/ dropjet (Selective Solder) | 26 November, 2019

we're using the Balverzinn Cobar 390-RX-HT and it wery good for wave and selective soldering and he can support a verry high temperatures

reply »

#83837

What flux are you using for spray/ dropjet (Selective Solder) | 29 November, 2019

Have used Interflux 2005C in a Ersaflow 3-45 and happy with the results

reply »

#83838

What flux are you using for spray/ dropjet (Selective Solder) | 29 November, 2019

flux my leave a white residues even after cleaning, when we want to select a flux for our Ersa Ecoslect we tryed a varity of fluxes (including the IF2005C) and we decide to use the Cobar 390-RX-HT because he gaved us the best results in soldering and cleaning

reply »

#83868

What flux are you using for spray/ dropjet (Selective Solder) | 4 December, 2019

We use the flux Cobar 94-SEL with excellent results. It is a special flux for selective soldering process. When the temperature of the board with flux (preheating or during soldering) reach more 130°C, the rests of flux are deactivated (no more dangerous).

reply »