solder mask peel off

Views: 671

#83779

solder mask peel off | 20 November, 2019

Hi, i'm facing solder mask peel off but limited to the solder defined pad only(opening area). no peel off on the other area and it happened on electroless nickel immersion gold finishing only. for other finishing is not affected. kindly advise if you ever encounter similar issue