Dear Team, We are facing open solder issue in a sensor comp... - Dec 27, 2019 by Ameen
Can you describe the failure mode of the soldering defect, i... - Dec 27, 2019 by Steve Thomas
Hi , Thanks..., Its "not wetting the pads sufficientl... - Dec 27, 2019 by Ameen
Yes we have tried with low soak with longer reflow and high ... - Dec 27, 2019 by Ameen
We switched to a REL0 T3 paste, Amtech LF-4300. It wets the ... - Dec 27, 2019 by Steve Thomas
Do you have clear picture show how it looks like solder open... - Dec 31, 2019 by sssamw
Let's stay away from the PCB and process for a while. This c... - Dec 31, 2019 by Evtimov
Hi Team, Thanks a lot for the valuable suggestions. Sorry ... - Jan 08, 2020 by Ameen