Looking for CTE and young's modulus values for aluminum backed PCB for solder joint predictions. The data sheets are a bit sparse, and the weighted average method somehow doesn't feel appropriate.

Any advice is welcome.

Thanks!

This message was posted via the Electronics Forum @ SMTASMTA

reply »


SMTA-Dave

#85064

Metal Clad PCB Mechanical Properties | 24 June, 2020

The typical CTE below Tg is 40 ppm/K and 110 above Tg ppm/K. The typical modulus is 16 Gpa