Part drop after reflow

Views: 880

#85096

Part drop after reflow | 26 June, 2020

Hi,

I am having a issue that SMT nut drop after reflow. The solder height all in specifications. Had tried adding flux inand the solder paste. But shows no improvement. Is the nut easily oxidize? Can anyone help me on this?

reply »

#85098

Part drop after reflow | 26 June, 2020

Hi Indhu,

It could be multiple reasons but probably one root cause. metal nut might require reflow profile change- you need to check it with SMT reflow profiler. the part might be oxidized - you can check solderability or try to solder part using a hand heat gun.

does the part mount on the bottom side and drop off during second side reflow?

cheers, victor

reply »

#85105

Part drop after reflow | 27 June, 2020

Hi Victor,

The part drop after the first side reflow itself. The part seems like didn't catch solder.

reply »

#85106

Part drop after reflow | 27 June, 2020

Hi Indhu,

Kindly check the data sheet of the part for Reflow details and what type of past is been used for Reflow?

reply »


SMTA-Davandran

#85107

Part drop after reflow | 27 June, 2020

Hi Indhu,

Check for solder paste height. Please manually add solder, mount component and reflow.