PCB Cleaning Challenges. | 24 July, 2020

Hello all,

We have a new model running upon analysis I found one challenge while cleaning the send side boards.

We have a thru hole in top where it's bottom ends are covered inside the shield.

Operator find difficult to clean as it has high chance to affect the bottom side component.

Kindly provide your valuable suggestions on how to clean this.

Any equipment available like vaccum method to remove the paste in via hole.

Refer the attached image for understanding.

Attachments:

reply »

#85357

PCB Cleaning Challenges. | 31 July, 2020

If any one can help. That would be much appreciated.

reply »

#85363

PCB Cleaning Challenges. | 3 August, 2020

Please try to use the steam aging tester and make a try !

When the water temp up to +100℃, Put your new model into the water tank.

This +100℃ hot and steam water may remove the paste in via hole. Thank you.

https://www.wewontech.com/steam-aging-test/

reply »

#85364

PCB Cleaning Challenges. | 3 August, 2020

Thanks for your response Caroline Yuanh,

I am speaking about one side complete board and we have MIC this will damage the mic.

reply »

#85370

PCB Cleaning Challenges. | 3 August, 2020

The usual accepted process would be to assemble and clean the board per the usual process, then install the shield with no-clean flux/solder.

Cheers, ..rob

reply »

#85372

PCB Cleaning Challenges. | 3 August, 2020

Thanks for your response.

Current I have implemented one process which is good with my current resources for cleaning

Thank you.

reply »

#85376

PCB Cleaning Challenges. | 4 August, 2020

Dear Srini: We have PCB cleaning machine that maybe can help you. We have been producing the SMT machines and intelligent equipment for many years, integrated Design, R&D, Production, Sales and Technical Service. What products we manufactured are: SMT Printer/Stencil Printer/Solder Paste Printer, Pick and Place Machine, SPI/AOI, Reflow Oven, Wave Soldering, Coating Machine, Glue Dispenser, Plug-in Machine, Laser Marker, Laser Soldering Machine, X-ray, Loader/Unloader, and Conveyor etc. On the other hand, we are the agency of: HANWHA (SAMSUNG) Chip Mounter and Pick&Place Machine, HELLER, PEMTRON, SAKI etc., and dedicated to provide the customers with professional and comprehensive one-stop solutions of the electronic assembly line. Any inquiry would be appreciated by Mobile/WeChat: 0086 13063047785 or scan my WeChat QR code. Yours sincerely Wellman Rau Senior Manager International Business Dept. Mobile/Wechat/WhatsApp: +86 130 6304 7785 Skype: wellmanrau@yeah.net">wellmanrau@yeah.net Email: wellman@htgdsmt.com">wellman@htgdsmt.com ; wellmanrau@yeah.net">wellmanrau@yeah.net Shenzhen HTGD Intelligent Equipment Co., Ltd. Website: http://www.htgdsmt.com" target="_blank">http://www.htgdsmt.com

Attachments:

reply »

#85378

PCB Cleaning Challenges. | 4 August, 2020

Hi wellman Rau,

Thanks for your response.

We do have cleaner M/C. My case was having challenges to clean.

Got a simple solution now.