Gold mitigation

Views: 611

#85353

Gold mitigation | 30 July, 2020

Is there a way I can inspect for gold embrittlment.

reply »

#85354

Gold mitigation | 31 July, 2020

The down and dirty method is to pop a part off using mechanical leverage.

Otherwise you may be able to see it if you have a good Xray or CT.