Stencil design | 17 September, 2020

Hi All, Is there any specific control for solder height and volume? Such as 3 mil what will be the height and volume upper and lower limit?

This message was posted via the Electronics Forum @ SMTASMTA

reply »

#85649

Stencil design | 17 September, 2020

For height, I start +-2mil usually. For 3mil stencils, my lower limit starts at 1.5mil, upper is 5. If the area is chem ethed, I normally add .5 to the stencil height. My default volume is 60 - 160%. Then print specs are adjusted till I see fit, then the inspection tols depending on the board and footprints. In my experience, there is only so much that can be done with poorly designed, cheap boards. The well designed, quality made boards almost always print within those default parameters for me.

reply »


SMTA-64386317

#85651

Stencil design | 18 September, 2020

Thank you for your input.

This message was posted via the Electronics Forum @ SMTASMTA

reply »

 Reflow System

Reflow Oven