Ferrite Core cracks

Views: 1689

#86475

Ferrite Core cracks | 1 April, 2021

Is there a standard that gives criteria for cracks in Ferrite Cores? I have reviewed Jstd-oo1 G and IPC 610 G and do not see a specific reference to Ferrites. Thanks for your help

reply »

#86477

Ferrite Core cracks | 2 April, 2021

IEC 63093-1:2020 - Ferrite cores - Guidelines on dimensions and the limits of surface irregularities - Part 1: General specification

reply »

#86478

Ferrite Core cracks | 2 April, 2021

thanks

reply »