Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7141
Hello all, Can anyone advise if any standard covers ENIG pla... - Nov 07, 2022 by Evtimov
ENIG boards have low shelf life as oxidation starts showing ... - Nov 09, 2022 by Micropak
If they are vacuumed and they approach 6months or 1 year mar... - Nov 09, 2022 by Evtimov
Probably preform some sort of solderability evaluation on th... - Nov 10, 2022 by dontfeedphils
The G in ENIG is gold. It does not oxidise. Either you are t... - Nov 10, 2022 by Stephen
The solderability shelf life of ENIG is related almost entir... - Nov 10, 2022 by SMTA-64386598 SMTA
So if you stored them in a nitrogen cabinet then you would r... - Nov 10, 2022 by Stephen
SMTA-643865, this is great information. I recently found onl... - Nov 11, 2022 by Evtimov
I would certainly test the boards but from our experience, t... - Nov 11, 2022 by kumarb
Thank you Stephen... I also mistaken it with Immersion Silve... - Nov 12, 2022 by Micropak
kumarb would you just check PCBs for solderability or would ... - Nov 14, 2022 by Evtimov
Yes, solderbility. I recall one case of a vendor we met at a... - Nov 15, 2022 by kumarb
" so I wander what can I do to save them?" The boa... - Nov 16, 2022 by Stephen
I need to back it up with a something like IPC standard. It ... - Nov 17, 2022 by Evtimov
You might be able to create a process that involves testing ... - Nov 17, 2022 by Stephen
Hello Evtimov, sorry...just saw post as I was looking throug... - Jan 06, 2023 by SMTA-64419298 SMTA