#9940

Electrum bar solder | 25 August, 1999

Has anyone used bar solder from a company called "Electrum Inc." What kind of results did you have?

reply »

#9941

Re: Electrum bar solder | 25 August, 1999

| Has anyone used bar solder from a company called "Electrum Inc." | What kind of results did you have? | | Hammer: Try:

Electrum Recovery Works 827 Martin St Rahway, NJ 07065 908-396-1616 800-622-1192 Canada 800-535-1192 Fax: 908-396-9390 John Silva,VP Metal

Ta

Dave F

reply »

Brian

#9942

Re: Electrum bar solder | 26 August, 1999

| | Has anyone used bar solder from a company called "Electrum Inc." | | What kind of results did you have? | | | | | Hammer: Try: | | Electrum Recovery Works 827 Martin St Rahway, NJ 07065 908-396-1616 800-622-1192 Canada 800-535-1192 Fax: 908-396-9390 John Silva,VP Metal

Never heard of it, but if it is recycled solder, I'd be VERY wary about putting it in a soldering machine. It could be OK but it might ruin your 350 kg or whatever of solder you have in it. I would want a very strict guaranteed analysis of all impurities and this includes non-metallic ones, including dross before I would even consider adding just 1 kg.

Caveat emptor | | Ta | | Dave F |

reply »

Brian

#9943

Re: Electrum bar solder | 26 August, 1999

| | Has anyone used bar solder from a company called "Electrum Inc." | | What kind of results did you have? | | | | | Hammer: Try: | | Electrum Recovery Works 827 Martin St Rahway, NJ 07065 908-396-1616 800-622-1192 Canada 800-535-1192 Fax: 908-396-9390 John Silva,VP Metal | | Ta | | Dave F | Dave

Sorry I split your message!