BGA Non-wet (head in pillow)

Scott Welle

#2451

BGA Non-wet (head in pillow) | 15 November, 2000

We are having non-wet (head in pillow) problems with Altera 484's similar to the problems discussed on 10/27 timeframe. Need contacts to those people having similar problems. Will those who had problems with Motorola 357 (ref Chris and Glenn on 10/27) or others please contact me ASAP with E-mail. scott.a.welle@honeywell.com