chem etching

john

#14791

chem etching | 4 August, 1998

We are looking for chem etching equipment. Does anyone know where I can find chem / laser systems?

reply »

Ben Salisbury

#14797

Laser systems | 5 August, 1998

| We are looking for chem etching equipment. | Does anyone know where I can find chem / laser | systems? AB Lasers (805) 274-0408 Kentek 800-432-2323 AB has a complete line of laser marking systems and Kentek does new and used equipment, baoth are fairly decent companies to deal with. -Ben

reply »

Dave F

#14793

Re: chem etching - Used For What? | 5 August, 1998

| We are looking for chem etching equipment. | Does anyone know where I can find chem / laser | systems? John: What is your planned end-use of such a system? 1 Making labels / labeling parts 2 Making SMT stencils 3 Something else

reply »

Ben Salisbury

#14794

Re: chem etching - Used For What? | 5 August, 1998

| | We are looking for chem etching equipment. | | Does anyone know where I can find chem / laser | | systems? | John: What is your planned end-use of such a system? | 1 Making labels / labeling parts | 2 Making SMT stencils | 3 Something else How about high tech tatoos...heh...sorry, just been one of those days. -Ben

reply »

john

#14795

chem etching for stencils | 5 August, 1998

Probably should have been more specific. We want to do some stencil etching. Mainly for prototype work nothing too high volume. Thanks, Oh yeah, (Ben) and maybe a tattoo here and/or there.. Ha ha ...

reply »

Wayne

#14792

Re: chem etching | 6 August, 1998

John: You can also check out: Lumonics Control Laser Both have CO2 laser systems that might be of interest to you. Wayne

reply »

Alex Ondi

#14796

Re: chem etching for stencils | 12 August, 1998

:Try American Plating Systems for Chem Etch Equipment, LPKF (Germany)for Laser cutting systems (A Laser in Oregon is the local distributor for LPKF), Lumonics is another option for Laser cutting systems. Probably should have been more specific. | We want to do some stencil etching. | Mainly for prototype work nothing too high volume. | Thanks, | Oh yeah, (Ben) and maybe a tattoo here and/or | there.. | Ha ha ...