Several online PCB fabrication quote forms offer SMOBC as a surface finish along with HASL, Ni/AU, etc. How does one specifify SMOBC for traces and untented vias, and elctroless Ni/Au for smt pads? Are these processes mutually exclusive? Or can I get both as desired?

reply »

#2763

Re: PCB Surface Finishing | 12 October, 2000

Actually they are complimentary. SMOBC describes how the solder mask shall be applied (but not the type, surface finish, color, etc). The other terms describe the type of surface protective finish applied to the solderable surfaces. You need to specify both attributes. You can find more information in the archives.

reply »

Facility Closure

Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes