Contaminated Pads

Jason Wraight

#2978

Contaminated Pads | 20 September, 2000

I am sure that this is a problem that will never be solved, but something that I am seeing in increased numbers. Often refered to as "Black Pads". After production, returns from the field coming back with contaminated pads under various components. They have a blackish tinge to them and solder will not adhere to them. I know that I am being very vague, but there is so much information surrounding this I hardly know where to start. Any ideas? Have already looked into the PCB manufacturing process, masking, baths, etc.

reply »

#2979

Re: Contaminated Pads | 20 September, 2000

Consider searching the SMTnet archives. There's 30+ postings for black and pads. Good luck.