Profile ISO Document | 8 January, 2002

I have recently purchased a datapaq 9000 and need to create an ISO document to use this device in my process. I will be using it for profiling new jobs for SMT and TH as well as monitoring the consistency of the oven performance. Before I create this painfull document is there anyone out there that already has. If so could I have a copy your document for a guide to creating my own.

Thanks

reply »

#18604

Profile ISO Document | 8 January, 2002

Look to 7530 �Guidelines for Temperature Profiling for Mass Soldering (Reflow and Wave)�. Obtain it from IPC http://www.ipc.org