Glass pack Diodes | 20 May, 2002

What is the recommended prep for a through-hole glass pack diode? Should a stand-off be used or can it lay flat on surface of the pcb?

This message was posted via the Electronics Forum @

reply »


RDR

#19983

Glass pack Diodes | 20 May, 2002

I have always installed them flush to board unless noted on assy. dwg.

Russ