wave profile

pzohbon

#20945

wave profile | 29 July, 2002

Does anyone know where to find information for wave temp profiling?

pzohbon

reply »

#20947

wave profile | 29 July, 2002

Look to: * Your flux supplier's recommendations to baseline your recipe [similar to using your paste supplier's recommendations for setting your reflow recipe] * 7530 'Guidelines for Temperature Profiling for Mass Soldering (Reflow and Wave)' for guidance * SMTnet Archives for additional tips