Specifying Surface finish on a BGA Module

David

#24324

Specifying Surface finish on a BGA Module | 28 April, 2003

Can anyone help me with a problem I am encountering on specifying the surface finish on a new BGA System in Package module. So far I have been advised to look at a palladium / nickel / gold solution but does that have any advantages over nickel / gold process. It seems more costly.

Thanks

This message was posted via the Electronics Forum @

reply »

#24371

Specifying Surface finish on a BGA Module | 30 April, 2003

ENIG is a common solderability protection on BGA packages.

Pd/Ni/Au while more expensive could have advantages over ENIG in the following area: * Allow both gold and aluminium wire bonding * Better solder resist compatibility (63�C max) * Might take multiple solder operations better

reply »