Hi Need some help here. Anybody got the recommended profile for Sn50/Pb50 solder paste. Thanks.

reply »

#25167

Reflow profile for Sn50/Pb50 solder paste | 15 July, 2003

We don't use Sn50, but if we did, we'd use our paste supplier's recommendation as the starting point for developing our reflow recipe.

reply »

MA/NY DDave

#25168

Reflow profile for Sn50/Pb50 solder paste | 15 July, 2003

Hi,

What are you soldering with Pb50Sn50?

YiEngr, MA/NY DDave

This message was posted via the Electronics Forum @

reply »

Thomas

#25180

Reflow profile for Sn50/Pb50 solder paste | 15 July, 2003

It is for an evaluation run for wafer bumping....Well guys any recommendation for the profile ??

reply »

Thomas

#25181

Reflow profile for Sn50/Pb50 solder paste | 15 July, 2003

Hi Dave, I saw many of your outstanding comments and postings. Can you save me this time on the profile recommendation ??

reply »


RDR

#25188

Reflow profile for Sn50/Pb50 solder paste | 16 July, 2003

Who is the paste manufacturer? They are the ones who can tell you what to run.

reply »

MA/NY DDave

#25189

Reflow profile for Sn50/Pb50 solder paste | 16 July, 2003

Hi,

I agree with everyone else talk to the Mfg and ask for their recommended profiles. They should know the heating and the cooling profiles.

If you really want to do this yourself you are going to have to run several experiments to determine just how the flux works and at what temperature. Do you need to hold it at temperature (soak) or can you ramp.