Solder paste tube storage

#25287

Solder paste tube storage | 29 July, 2003

Does anyone out there have any documentation supporting the storage of 1300 gram tubes on the tip. Thanks in advance!

reply »

blnorman

#25331

Solder paste tube storage | 1 August, 2003

Kester recommends that we store our 1400 gm tubes on the tip. Our documentation is based on their recommendation. The Alpha past we used was stored horizontally, but that was because the flux readily separated from the metal.

reply »