PTH hole size for soldering wires


DCK

#27136

PTH hole size for soldering wires | 5 February, 2004

We have recent customer asking for PCB's PTH hole size related to soldered wire AWG 18-26. Please kindly advise any international standard for captioned issue.

Thanks!

reply »

#27140

PTH hole size for soldering wires | 5 February, 2004

IPC-2222 - Sectional Design Standard For Printed Board For Organic Printed Boards, Table 9-3 � Plated Through Hole Diameter To Lead Diameter Relationships will give you the standard information you require.