BGA standards

Billy

#3868

BGA standards | 9 June, 2000

Hi, Does anyone know where I can find some sort of standard for BGA's? We have done quite a bit of BGA rework and some of the results are less than spectacular when viewed with the X-ray machine. For example, on a lot of the boards the ball seems to have completely disappeared, and I have nothing with which to gauge these boards against.

Any help would be appreciated, bw