Hi Has anyone see a defect,where after one pass over the ... - Sep 14, 2004 by
Adam, Is your fluxer giving you good coverage into the ho... - Sep 14, 2004 by
I would need a little more information to be able to rule ou... - Sep 14, 2004 by
I have chceked the fluxing application, I seem to be getting... - Sep 15, 2004 by
No blow-holes, only minimum solder fillets. Adam ... - Sep 16, 2004 by
Hi Adam, What machine are you running? Rob. ... - Sep 16, 2004 by Rob
Rob The machine is SEHO MWS8240, Fitted with a foam fluxe... - Sep 17, 2004 by
Adam, If you use the chipwave on that board, eliminate th... - Sep 17, 2004 by Patrick Bruneel
Patrick Tried That, unfortunately it didn't work. Adam... - Sep 20, 2004 by
Hi Adam, We had a reverse of the previous - if we didn't ... - Sep 20, 2004 by Rob
Just a thought, Solder flows to leads of parts and will tend... - Sep 22, 2004 by Paul pmd
First, Your flux is no good replace it. second, Check for pr... - Sep 27, 2004 by Grayman
Adam, I would first check hole to lead sizes on the comp... - Sep 28, 2004 by