Cleanliness Testing Samples - What to Use?

HOSS

#30827

Cleanliness Testing Samples - What to Use? | 4 October, 2004

We are trying to deploy an Ionograph cleanliness tester and wanted to know what others are using as a standard test sample. My desire is to run the test on a weekly basis using the same medium complexity assembly. We plan to use the testing as a process monitoring tool. To do this we need the test parameters to be the same each time we test.

Because we are a CM, we rarely run the same assembly weekly or even monthly. Any input appreciated.

reply »

#30838

Cleanliness Testing Samples - What to Use? | 4 October, 2004

We know SIR coupons are not ROSE coupons, but coupon boards are: * IPC-B-24 (copper and HASL, FR-4 and polyimide) * IPC-B-36 (bare copper and HASL, FR-4 and polyimide) * IPC Phoenix board (bare copper, FR-4) * IPC-B-25A (FR-4, bare copper only)

reply »

blnorman

#30905

Cleanliness Testing Samples - What to Use? | 8 October, 2004

Since you are using an Ionograph you need to use IPC-TM-650 method 2.3.25, static method. The test method is free on the IPC website.

You'll need to get your customer to give you an acceptable cleanliness level to test to.

reply »