#31311

Wash machine settings | 10 November, 2004

Does anyone know where to find the guidelines to validate a pcb cleaning process (Water deionizing system)?

I appreciate your feedback.

Regards, Hiram

reply »

GS

#31369

Wash machine settings | 13 November, 2004

Hello,

very interesting informations you can find on:

- IPC-CH-65A Guidelines for Cleaning of Printed Board and Assemblies. - IPC-AC-62A Aqueous Post Solder Cleaning hand Book

GS

This message was posted via the Electronics Forum @

reply »

Shean Dalton

#31375

Wash machine settings | 15 November, 2004

Hello Hiram,

We are happy to be available for any questions you may not find answered in the good references G.S. provided.

Shean Dalton Austin American Technology www.aat-corp.com (+1) 512-335-6400

reply »

Hiram

#31381

Wash machine settings | 15 November, 2004

The information provided has been very helpful.