We do a lot of prototype work, builds occur days or months apart and moisture Absorption in IC's is a worry. I would like to bake, chuck in some silica gel and then seal or vac seal in an envelope. Does anyone have any experience of vacuum sealing waffle trays ? Do you know of any machine suppliers ? ( UK proffered )

Your help would be much appreciated. David

reply »

#4045

Re: Vacuum packaging | 23 May, 2000

David: Beyond the information on sealing components in the archives, look for information on protecting boards. Further, consider a dessicant cabinet, as an alternative. Sources are also in the archives. Good luck. Dave F