Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


DEK Pump Print

John S

#32354

DEK Pump Print | 31 January, 2005

We have a line using the DEK Pump Print process. We use a 3mm plastic stencil and print adhesive through it. The adhesive we use is Heraeus 955. We've struggled with adhesive contaminating the pads of our smaller components. The deposit isn't on the pad, and there is no visible squeeze out, but in changing the stencil to move the glue as far away as possible, the problem goes away. Recent constraints have put me back into this again.

Can anyone recommend a good adhesive for this process? Has anyone experienced anything similar? It seems like a layer of "stuff" may be squeezing out from the holes, but it isn't easy to detect.

Thanks John

reply »

Chunks

#32355

DEK Pump Print | 31 January, 2005

Not to put Heraeus down - but we experienced the same thing from time to time. We finally found out it was the humidity in building. The higher humidity would cause the bleed out of this adhesive. We switched to Loctite and the problem went away.

reply »

SMT spare parts - Qinyi Electronics

Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes