we are having problem with the flipchip sticking to the tape...
- Feb 18, 2005
by
Potential causes are:
* Static charge [get a deionizing fan...
- Feb 19, 2005
by
davef
Agree with Davef. Smaller the chip, more the static charge. ...
- Feb 21, 2005
by
ABHI
Thanks for your help. We try the de-ionizer fan, helps some ...
- Feb 21, 2005
by
need help