What test is applicable to check for QFN package with NiPdAu leadframe if leads/pad are solderable? what are the options other than dip and look solderability testing?

Thanks,

reply »

#33895

QFN Solderability | 26 April, 2005

You could use a meniscograph to test for wetability. It will give you a tangible measure of the solderability of the component. Just do a net search for 'meniscograph'.